性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
比重 | ASTMD792 | 1.14 | g/cm3 | |
熔流率(熔体流动速率)(190°C/10.0kg) | ASTMD1238 | 20to50 | g/10min | |
拉伸模量(注塑) | ASTMD412 | 8.96 | MPa | |
弯曲模量(注塑) | ASTMD790 | 10.3 | MPa | |
泰伯耐磨性 | ASTMD1044 | 20.0 | mg | |
Abrasion-DIN | DIN53516 | 45 | mm3 | |
弹性体 | TestMethod | NominalValue | Unit | |
拉伸应力(100%应变) | ASTMD412 | 5.72 | MPa | |
拉伸应力(300%应变) | ASTMD412 | 17.9 | MPa | |
抗张强度 | ASTMD412 | 26.2 | MPa | |
伸长率(断裂) | ASTMD412 | 600 | % | |
撕裂强度2 | ASTMD624 | 80.6 | kN/m | |
压缩永久变形 | 23°C,22hr | ASTMD395B | 20 | % |
压缩永久变形 | 70°C,22hr | ASTMD395B | 45 | % |
肖氏硬度(邵氏A) | ASTMD2240 | 75 | ||
玻璃转化温度 | InternalMethod | -48.0 | °C | |
维卡软化温度 | ASTMD1525 | 80.0 | °C | |
SofteningPoint-DMA | InternalMethod | 60 | °C | |
UL阻燃等级 | 1.2mm | UL94 | V-2 | |
UL阻燃等级 | 3.0mm | UL94 | V-2 | |
UL阻燃等级 | 0.9mm | UL94 | V-0 | |
UL阻燃等级 | 1.1mm | UL94 | V-0 |
TPU聚醚 1175AW塑料供应商,长期销售德国巴斯夫生产的TPU聚醚原料,以上是“TPU聚醚 Elastollan® 1175AW”塑胶料的物性表参数.近期代理商可转仓交易:沙伯基础 PP SABIC® STAMAX 20YM240 resin 填料,长玻璃纤维,20%填料按重量.
法国阿科玛 PVDF Kynar® 370
德国巴斯夫 TPU聚脂 Elastollan® C95A10
美国塞拉尼斯 TPU Celstran® TPU-GF60-01 填料,长玻璃纤维,60%填料按重量.
美国Teknor Apex TPE Telcar® TL-3050-88
美国普立万 TPE Versaflex™ 9570-9 优良外观,良好的着色性,良好的流动性,注射成型
中国深圳盛嘉伦 TPE Gallonprene® GP540-7502(n)F 高弹性,阻燃性,无卤,优良外观,型材挤出成型,挤出 电线电缆应用,型材,管件
日本三菱 SEBS tefabloc® TO 228
美国埃克森美孚化工 PP弹性体 Vistamaxx™ 6502 复合
意大利API EVA apizero® AZ FC 200 可交联,注射成型 玩具
美国塞拉尼斯 PPS Fortron® 4332L6
美国Polymics PEI Pyramid™ PEI II2230 填料,碳纤维增强材料,20%填料按重量.
● TPU聚醚 意大利COIM LARIPUR LPR 5760
良好耐磨损性,耐化学性良好,低温下的柔性,耐气候影响性能良好,注射成型
● TPU聚醚 中国山东奥邦化工 Shandong Aobang TPU-Polyether 90-A
● TPU聚醚 美国Biomerics Quadraflex ALE-93A-B30
● TPU聚醚 意大利COIM LARIPUR LPR 5260
低温下的柔性,耐化学性良好,耐气候影响性能良好良好,耐磨损性,挤出,注射成型
● TPU聚醚 美国路博润 Estane 58630 TPU