| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
| 熔体流动速率 | 190℃/2.16kg | ASTM D-1238 | 0.45 | g/10min |
| VA含量 | 13.5 | wt% | ||
| 薄膜厚度 | 38.1 | um | ||
| 1%正割模量(TD) | 38.1um | ASTM D-882 | 91 | MPa |
| 1%正割模量(MD) | 38.1um | ASTM D-882 | 90.3 | MPa |
| 拉伸屈服强度(MD) | 38.1um | ASTM D-882 | 6.62 | MPa |
| 拉伸屈服强度(TD) | 38.1um | ASTM D-882 | 5.52 | MPa |
| 拉伸断裂强度(MD) | 38.1um | ASTM D-882 | 30.5 | MPa |
| 拉伸断裂强度(TD) | 38.1um | ASTM D-882 | 29.8 | MPa |
| 屈服伸长率(TD) | 38.1um | ASTM D-882 | 16 | % |
| 屈服伸长率(MD) | 38.1um | ASTM D-882 | 18 | % |
| 断裂伸长率(TD) | 38.1um | ASTM D-882 | 600 | % |
| 断裂伸长率(MD) | 38.1um | ASTM D-882 | 300 | % |
| 埃尔曼多夫撕裂强度(TD) | 38.1um | ASTM D-1922 | 130 | g |
| 埃尔曼多夫撕裂强度(MD) | 38.1um | ASTM D-1922 | 92 | g |
| 落镖冲击 | 38.1um | ASTM D-4272 | 570 | g |
| 脆化温度 | ASTM D-746 | <-76 | ℃ | |
| 维卡软化温度 | ASTM D-1525 | 80 | ℃ | |
| 熔点 | DSC | 94.4 | ℃ | |
| 氧气传输速率 | 23℃,38.1um | ASTM D-3895 | 8900 | cm3/m2/24hr |
| 水蒸气传输速度 | 38℃,38.1um | ASTM F-372 | 85 | g/m2/24h |
| 光泽度 | 45°,38.1um | ASTM D-2457 | 88 | |
| 透明度 | 38.1um | ASTM D-1746 | 78 | |
| 雾度 | ASTM D-1003 | 1.5 | % | |
EVA UE672317塑料供应商,长期销售利安德巴塞尔生产的EVA原料,以上是“EVA UE672317”塑胶料的物性表参数.近期代理商可转仓交易:印度Supreme HIPS SH 820 与食物接触的可接受的,良好的耐冲击性,高光泽,可喜的表面形貌 电器元件,玩具
日本旭化成 PP P6-30FG-0153 玻纤增强30%
日本宝理 PBT 2016 阻燃
北欧化工 PP BA202E 嵌段共聚物的特点,超高分子量,低流量,超高耐冲击 波纹管
利安德巴塞尔 PP PP41BW01 均聚注塑
上海狄斯玛 PBT D2500L 高流动性 微型马达骨架
美国福禄 PP TPP20AJ34NA 滑石填料,21%填料按重量,均聚物,热稳定性
澳大利亚Marplex PA6 GRC6L UHS 抗撞击性,抗紫外线,热稳定性,冲击调节器
中原石化 PP D60P 均聚物,挤塑 压力管,管件,板材,条,带
美国杜邦 PA66 51HSL NC001 (Dry) 玻纤增强,注塑
三菱工程塑料 PC LGS-2430M 耐磨,增强,纤维
美国Spartech HIPS SC2-1090 尺寸稳定性良好,经润滑,抗撞击性良好,可加工性良好,良好的柔韧性,耐化学性良好,热稳定性良好,韧性良好,中等粘性 电气/电子应用领域,汽车领域的应用,工业领域,体育用品
美国诺瓦 ABS/PC NC-8384LM BK 注塑
德国巴斯夫 TPU Konz134/F 射出,挤出
美国TPC PA6 IM B 热稳定,导电 导电,热稳定,抗冲击改进型,润滑