高强度,清晰度,高,良好的开裂抵抗 | |
包装,双向拉伸薄膜 | |
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
摩擦系数 | 与金属-动态 | ASTMD1894 | 0.17 | |
摩擦系数 | 与自身-动态 | ASTMD1894 | 0.44 | |
薄膜厚度-经测试 | 8.1 | um | ||
割线模量 | MD:8.1um | ASTMD882 | 2760 | MPa |
割线模量 | TD:8.1um | ASTMD882 | 1900 | MPa |
抗张强度 | MD:断裂,8.1um | ASTMD882 | 241 | MPa |
抗张强度 | TD:断裂,8.1um | ASTMD882 | 290 | MPa |
伸长率 | MD:断裂,8.1um | ASTMD882 | 90 | % |
伸长率 | TD:断裂,8.1um | ASTMD882 | 75 | % |
透氧率(25°C,8.1um) | ASTMD3985 | 2.1 | cm3mm/m2/atm/24hr | |
水气透过率(8.0um,38°C,100%RH) | ASTMF1249 | 530 | gmm/m2/atm/24hr | |
薄膜厚度-经测试 | 8.1 | um | ||
割线模量 | MD:8.1um | ASTMD882 | 2760 | MPa |
割线模量 | TD:8.1um | ASTMD882 | 1900 | MPa |
抗张强度 | MD:断裂,8.1um | ASTMD882 | 241 | MPa |
抗张强度 | TD:断裂,8.1um | ASTMD882 | 290 | MPa |
伸长率 | MD:断裂,8.1um | ASTMD882 | 90 | % |
伸长率 | TD:断裂,8.1um | ASTMD882 | 75 | % |
透氧率(25°C,8.1um) | ASTMD3985 | 2.1 | cm3mm/m2/atm/24hr | |
水气透过率(8.0um,38°C,100%RH) | ASTMF1249 | 530 | gmm/m2/atm/24hr | |
光泽度(20°,8.13um) | ASTMD2457 | 150 | ||
雾度(8.13um) | ASTMD1003 | 2.5 | % |
PA6 800塑料供应商,长期销售美国Honeywell生产的PA6原料,以上是“PA6 Capran Medallion® 800”塑胶料的物性表参数.近期代理商可转仓交易:美国Techmer PBT Plaslube® PC / PBT IM 5230 抗撞击性高,注射成型
意大利Vamp Tech PC DENIBLEND F 抗撞击性良好
德国Almaak PC Anjacom® 050/75S 注射成型
美国KMI PBT PrimoTek KM6090
韩国LG化学 PBT Lupox® GP2306FB 阻燃性,注射成型 电气/电子应用领域
美国杜邦 PBT Crastin® LW9330 BK851 填料,玻璃纤维增强材料,30%填料按重量.
沙伯基础 PA66 LNP™ THERMOCOMP™ RX04515H compound
巴西Petropol PA66 Nypol® PA A3 G43 HS UV RH PRTA011 NR424 填料,玻璃纤维增强材料,43%填料按重量.
德国朗盛 PA66 Durethan® AKV 35 H3.0 000000
德国DimeLika PA66 CompaMid® PA 6.6 GF 25
德国巴斯夫 PA66 Ultramid® A3EG7 BK00564
日本东洋纺 PA66 GLAMIDE® T-656E 良好耐磨损性
意大利波利布兰德 PA6 Polimid B 50 GF 填料,玻璃纤维增强材料,50%填料按重量.
英国Jackdaw PA6 VITAMIDE® BI12BK6523 冲击改性
韩国可隆 PA6 KOPA® KN133G20HIBK 填料,玻璃纤维增强材料,20%填料按重量.
● PA6 美国Adell BT-17
玻璃纤维增强材料33%。特点:改良撞击性。
● PA6 土耳其EMAS EMLON 6 GBR 20 FR V0
填料:玻璃珠。
● PA6 斯洛伐克Plastcom SLOVAMID 6 GF 35
● PA6 台湾南亚 2210G9
45%玻纤增强
● PA6 美国Teknor Apex MDF2
玻璃纤维增强材料, 30% 填料按重量、良好的表面光洁度、热稳定性