性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
比重 | ——2 | ASTMD792 | 1.35 | g/cm3 |
比重 | ——3 | ASTMD792 | 1.36 | g/cm3 |
吸水率 | 24hr,1.57mm | ASTMD570 | 2.0 | % |
吸水率 | 24hr,3.18mm | ASTMD570 | 1.2 | % |
吸水率 | 24hr,12.7mm | ASTMD570 | 0.74 | % |
抗张强度 | 流量:1.57mm | ASTMD638 | 88.9 | MPa |
抗张强度 | 横向流量:1.57mm | ASTMD638 | 55.8 | MPa |
抗张强度 | 流量:3.18mm | ASTMD638 | 93.8 | MPa |
抗张强度 | 横向流量:3.18mm | ASTMD638 | 68.9 | MPa |
弯曲强度 | 1.57mm4 | ASTMD790 | 147 | MPa |
弯曲强度 | 1.57mm5 | ASTMD790 | 110 | MPa |
弯曲强度 | 3.18mm4 | ASTMD790 | 122 | MPa |
弯曲强度 | 3.18mm5 | ASTMD790 | 105 | MPa |
弯曲强度 | 12.7mm4 | ASTMD790 | 121 | MPa |
弯曲强度 | 12.7mm5 | ASTMD790 | 99.3 | MPa |
压缩强度 | 1.57mm6 | ASTMD695 | 64.1 | MPa |
压缩强度 | 1.57mm7 | ASTMD695 | 63.4 | MPa |
压缩强度 | 3.18mm6 | ASTMD695 | 173 | MPa |
压缩强度 | 3.18mm7 | ASTMD695 | 170 | MPa |
压缩强度 | 3.18mm8 | ASTMD695 | >310 | MPa |
压缩强度 | 12.7mm6 | ASTMD695 | 84.8 | MPa |
压缩强度 | 12.7mm8 | ASTMD695 | >310 | MPa |
悬壁梁缺口冲击强度9 | 横向流量:1.57mm | ASTMD256 | 47 | J/m |
悬壁梁缺口冲击强度9 | 横向流量:3.18mm | ASTMD256 | 46 | J/m |
悬壁梁缺口冲击强度9 | 横向流量:12.7mm | ASTMD256 | 48 | J/m |
悬壁梁缺口冲击强度9 | 流量:1.57mm | ASTMD256 | 65 | J/m |
悬壁梁缺口冲击强度9 | 流量:3.18mm | ASTMD256 | 61 | J/m |
悬壁梁缺口冲击强度9 | 流量:12.7mm | ASTMD256 | 54 | J/m |
线形热膨胀系数 | 流动:3.18mm | 2.6E-5 | cm/cm/°C | |
线形热膨胀系数 | 横向:3.18mm | 2.2E-5 | cm/cm/°C | |
表面电阻率9 | 1.57mm | ASTMD257 | 2.2E+11 | ohms |
表面电阻率9 | 3.18mm | ASTMD257 | 1.6E+12 | ohms |
体积电阻率9 | 1.57mm | ASTMD257 | 4.4E+10 | ohmscm |
体积电阻率9 | 3.18mm | ASTMD257 | 1.1E+10 | ohmscm |
介电强度 | 1.57mm | ASTMD149 | 17 | kV/mm |
介电强度 | 3.18mm | ASTMD149 | 14 | kV/mm |
介电常数9 | 1.57mm,60Hz | ASTMD150 | 7.84 | |
介电常数9 | 1.57mm,1kHz | ASTMD150 | 6.81 | |
介电常数9 | 1.57mm,1MHz | ASTMD150 | 5.68 | |
介电常数9 | 3.18mm,60Hz | ASTMD150 | 9.49 | |
介电常数9 | 3.18mm,1kHz | ASTMD150 | 7.56 | |
介电常数9 | 3.18mm,1MHz | ASTMD150 | 6.15 | |
耗散因数9 | 1.57mm,60Hz | ASTMD150 | 0.22 | |
耗散因数9 | 1.57mm,1kHz | ASTMD150 | 0.79 | |
耗散因数9 | 1.57mm,1MHz | ASTMD150 | 0.043 | |
耗散因数9 | 3.18mm,60Hz | ASTMD150 | 0.27 | |
耗散因数9 | 3.18mm,1kHz | ASTMD150 | 0.093 | |
耗散因数9 | 3.18mm,1MHz | ASTMD150 | 0.046 | |
耐电弧性9 | 1.57mm | ASTMD495 | 143 | sec |
耐电弧性9 | 3.18mm | ASTMD495 | 148 | sec |
耐电弧性9 | 12.7mm | ASTMD495 | 63.0 | sec |
DielectricBreakdown9 | 1.57mm | ASTMD149 | 83000 | V |
DielectricBreakdown9 | 3.18mm | ASTMD149 | 73000 | V |
DielectricBreakdown9 | 1.27cm | ASTMD149 | 57000 | V |
UL阻燃等级 | 1.6mm | UL94 | HB | |
UL阻燃等级 | 3.2mm | UL94 | HB | |
UL阻燃等级 | 12.7mm | UL94 | V-0 | |
BondStrength9(1.27cm) | ASTMD229 | 880000 | g |
酚醛 LV355塑料供应商,长期销售美国Iten Industries生产的酚醛原料,以上是“酚醛 Resiten® LV355”塑胶料的物性表参数.近期代理商可转仓交易:沙伯基础 PP SABIC® PPcompound 9135A
日本三井 PP ADMER™ AT1404E 食品接触的合规性,良好粘结性,挤出 管道系统,粘合剂,非特定食品应用,食品服务领域,涂层应用
美国路博润 PP Carbo-Rite™ B-263
中国山东东辰 PP Shandong PA/PP PA66/PP 高耐热性,抗撞击性高,吸水低或不吸水,耐磨损性良好 轴承,家电部件,连接器,电气/电子应用领域
美国Honeywell PCTFE Honeywell PCTFE P3000TR 均聚物,耐化学性良好,阻隔树脂 工业应用,电气/电子应用领域
中国苏州奥斯汀 TPU聚脂 Texalan® 4 Series 472D 高弹性良好,耐磨损性,耐低温,抗撞击性高,高拉伸强度,耐油性能,压延,挤出,薄膜挤出,注射成型,共挤出成型,吹塑成型
日本CardioTech TPU聚醚 ChronoThane™ T 93A-B40
德国凯柏胶宝 TPE THERMOLAST® K TF6ADN (Series: FC/AD1/PS)
中国深圳盛嘉伦 TPE Gallonprene® GP550-6503 可焊接,高弹性,无卤,优良外观,抗微生物,挤出,型材挤出成型 型材,密封件
英国ELASTO SEBS Mediprene® A2 500550M
中国东莞顶塑 TPE Topolymer® 6200-T/C/A 鞋类,玩具
土耳其Elastron SEBS Elastron® G G400.A12.B 嵌段共聚物良好,耐磨损性,可粘结性,耐刮擦性,柔软,耐化学性良好,注射成型
日本东曹 EVA Melthene® -H 900W (White) 耐气候影响性能良好,抗溶剂性,良好粘结性,共聚物 涂层应用
美国KMI PSU KMI KM-P1700 NAT
土耳其Elastron SEBS Elastron® G G300.D50.B