性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
比重 | ASTMD792 | 1.35 | g/cm3 | |
吸水率(24hr,3.18mm) | ASTMD570 | 1.5 | % | |
抗张强度 | 流量:3.18mm | ASTMD638 | 101 | MPa |
抗张强度 | 横向流量:3.18mm | ASTMD638 | 89.6 | MPa |
弯曲强度 | 3.18mm2 | ASTMD790 | 136 | MPa |
弯曲强度 | 3.18mm3 | ASTMD790 | 129 | MPa |
压缩强度4(3.18mm) | ASTMD695 | 77.9 | MPa | |
悬壁梁缺口冲击强度5 | 横向流量:3.18mm | ASTMD256 | 29 | J/m |
悬壁梁缺口冲击强度5 | 流量:3.18mm | ASTMD256 | 31 | J/m |
RTIElec(3.2mm) | UL746 | 130 | °C | |
RTI(3.2mm) | UL746 | 130 | °C | |
介电强度(3.18mm) | ASTMD149 | 23 | kV/mm | |
介电常数5 | 3.18mm,1kHz | ASTMD150 | 5.84 | |
介电常数5 | 3.18mm,1MHz | ASTMD150 | 4.63 | |
耗散因数5 | 3.18mm,1kHz | ASTMD150 | 0.14 | |
耗散因数5 | 3.18mm,1MHz | ASTMD150 | 0.038 | |
耐电弧性5(3.18mm) | ASTMD495 | 21.0 | sec | |
相比耐漏电起痕指数(CTI)(3.18mm) | UL746 | 160 | V | |
高电弧燃烧指数(HAI)(3.18mm) | UL746 | >200 | ||
高电压电弧起痕速率(HVTR)(3.18mm) | UL746 | 12.0 | mm/min | |
热丝引燃(HWI)(3.18mm) | UL746 | 100 | sec | |
DielectricBreakdown5(3.18mm) | ASTMD149 | 50300 | V | |
UL阻燃等级(3.2mm) | UL94 | HB |
酚醛 115P塑料供应商,长期销售美国Iten Industries生产的酚醛原料,以上是“酚醛 Resiten® 115P”塑胶料的物性表参数.近期代理商可转仓交易:沙伯基础 PP SABIC® PP 90910
沙伯基础 PP LNP™ THERMOCOMP™ MB008S compound 填料,玻璃珠,40%填料按重量.
美国Techmer TPU HiFill® TPU GF30 填料,玻璃纤维增强材料,30%填料按重量.
中国山东美瑞新材 TPU聚脂 Mirathane™ E295U 管件,片材,薄膜,管道
新加坡R&P TPE RAYPRENE® NB221-S4051
美国普立万 TPE Versollan™ RU 2204X 良好耐磨损性,耐化学性良好,耐油性能,挤出,注射成型
美国Teknor Apex TPE Telcar® TL-1336G 挤出,注射成型 汽车外部装饰,垫圈,耐候性密封条,汽车外部零件,吹塑成型应用,通用,汽车内部零件,汽车领域的应用
斯洛文尼亚UTEKSOL SBS SOLPLAST TH 9000B
英国ELASTO SEBS Dryflex® 660600S
美国杜邦 EVA Elvax® 40L-03
韩国三养 PPS TRIPPS® 7A140
意大利Guarniflon PTFE Flontech® FT-BRR25-CF10-M5-1 填料,碳纤维增强材料,10%填料按重量,青铜填料,25%填料按重量,.
● 酚醛 日本住友酚醛塑料 RX 865M
填料:玻璃纤维增强材料。
● 酚醛 日本住友酚醛塑料 Durez 32340
● 酚醛 日本住友酚醛塑料 Vyncolit 4221XB
填料:玻璃纤维增强材料 矿物填料 纤维填料。
● 酚醛 美国Plastics Engineering Plenco 07321 (Compression)
填料:有机填料。
● 酚醛 美国ACCURATE Acculam Phenolkraft Paper XX/XXX