性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
比重 | ASTMD792 | 1.70 | g/cm3 | |
收缩率-流动 | ASTMD955 | 0.030 | % | |
洛氏硬度(R级) | ASTMD785 | 105 | ||
拉伸模量 | ASTMD638 | 19300 | MPa | |
抗张强度 | 屈服 | ASTMD638 | 148 | MPa |
抗张强度 | —— | ASTMD638 | 103 | MPa |
伸长率(断裂) | ASTMD638 | 1.0 | % | |
弯曲模量 | ASTMD790 | 15900 | MPa | |
弯曲强度 | —— | ASTMD790 | 145 | MPa |
弯曲强度 | 屈服 | ASTMD790 | 214 | MPa |
悬壁梁缺口冲击强度(3.18mm) | ASTMD256 | 64 | J/m | |
无缺口悬臂梁冲击(3.18mm) | ASTMD4812 | 270 | J/m | |
载荷下热变形温度(1.8MPa,未退火) | ASTMD648 | 321 | °C | |
RTIElec | 0.30mm | UL746 | 130 | °C |
RTIElec | 1.6mm | UL746 | 130 | °C |
RTIImp | 0.30mm | UL746 | 130 | °C |
RTIImp | 1.6mm | UL746 | 130 | °C |
RTI | 0.30mm | UL746 | 130 | °C |
RTI | 1.6mm | UL746 | 130 | °C |
介电强度 | ASTMD149 | 26 | kV/mm | |
介电常数(1MHz) | ASTMD150 | 3.60 | ||
耗散因数(1MHz) | ASTMD150 | 0.024 | ||
UL阻燃等级 | 0.30mm,BK,NC | UL94 | V-0 | |
UL阻燃等级 | 1.6mm,BK,NC | UL94 | V-0 |
LCP RTP 3407-4塑料供应商,长期销售美国RTP生产的LCP原料,以上是“LCP RTP 3407-4”塑胶料的物性表参数.近期代理商可转仓交易:美国Network Polymers TPE Softflex® 0809
土耳其Elastron SEBS Elastron® G G501.A60.B.PS 嵌段共聚物,良好粘结性,可粘结性,柔软,注射成型,挤出
美国RTP SEBS RTP 2700 S-40A MD NATURAL 注射成型
美国MPI EVA MARPOL® EVA 6055
丹麦UNIFLON PTFE Fluoroplex F 15 AZ 02 - GMP 填料,玻璃纤维增强材料,15%填料按重量.
美国RTP PSU RTP 900 P-1700 注射成型
德国爱彼斯 PPS TEDUR® L 9510-1 S 填料,玻璃纤维增强材料,40%填料按重量.泵件,机器/机械部件
美国RTP PEI RTP 2105 HF TFE 15 填料,玻璃纤维增强材料,30%填料按重量.
美国Techmer POM均聚 Plaslube® Actrn 润滑,自润滑,注射成型 轴承,衬套
美国RTP PEEK RTP 2288 HF 填料,碳纤维增强材料,45%填料按重量.
台湾台化 POM共聚 FORMOCON® FM350
美国Delta POM共聚 Delta ATR-2G50 填料,玻璃纤维增强材料,25%填料按重量.保护涂料,涂层应用,修复材料
美国Biomerics PC Quadrathane™ ALC-72D-B20
德国科思创 PC Bayblend® FR3010 IF
美国RTP PC RTP EMI 362 FR
● LCP 美国塞拉尼斯 Zenite 6130L
填料:玻璃纤维增强材料, 30% 填料按重量。
● LCP 美国塞拉尼斯 5115L
韧性良好
● LCP 泰科纳 MT1305
15%的玻璃纤维增强
● LCP 德国BARLOG plastics KEBAFLOW LCP MX130
填料:玻璃矿物, 30% 填料按重量。
● LCP 泰科纳 V400P
耐化学性良好,阻燃剂