| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
| 密度 | ASTMD1505 | 0.929 | g/cm3 | |
| 熔流率(熔体流动速率) | ASTMD1238 | 0.55 | g/10min | |
| 醋酸乙烯含量 | 7.5 | wt% | ||
| 薄膜厚度-经测试 | 32 | um | ||
| SecantModulus-1%Secant,MD(32um,BlownFilm) | ASTMD882 | 103 | MPa | |
| SecantModulus-1%Secant,TD(32um,BlownFilm) | ASTMD882 | 110 | MPa | |
| TensileStrength-MD(Break,32um,BlownFilm) | ASTMD882 | 24.1 | MPa | |
| TensileStrength-TD(Break,32um,BlownFilm) | ASTMD882 | 25.5 | MPa | |
| TensileElongation-MD(Break,32um,BlownFilm) | ASTMD882 | 380 | % | |
| TensileElongation-TD(Break,32um,BlownFilm) | ASTMD882 | 550 | % | |
| 落锤冲击(32um,吹塑薄膜) | ASTMD1709 | 480 | g | |
| 光泽度(45°,31.8um,吹塑薄膜) | ASTMD2457 | 74 | ||
| 雾度(31.8um,吹塑薄膜) | ASTMD1003 | 4.8 | % | |
| 补充信息 | TestMethod | NominalValue | Unit | |
| BlownFilmMeltTemperature2 | 182to204 | °C | ||
EVA EF575塑料供应商,长期销售美国华美化学生产的EVA原料,以上是“EVA ELEVATE™ EF575”塑胶料的物性表参数.近期代理商可转仓交易:日本旭硝子 氟橡胶 AFLAS® 150P
美国亨斯迈 TPU聚脂 IROGRAN® A 86 E 4486
芬兰Plasthill PLA Kareline® PLMS6040
日本住友酚醛塑料 酚醛 Durez® 33553
美国APS TPV Viprene™ G50D-32U-BLK 热稳定性,抗紫外线性能良好,良好的流动性,注射成型,挤出
美国Argotec TPU Argothane® TX2060
美国Advanced TPE DuraGrip® DGR 6220CL
台湾匹优 TPU聚醚 TPUCO® TPUE-UEH90 良好耐磨损性,耐水解性,耐磨损性良好,挤出 片材,管件,电线电缆应用,薄膜,传送机,管道
日本三菱 TPV Trexprene® A88BU
美国RTP SEBS RTP 2700 S-40A Z 注射成型
美国Infinity LTL PSU INSTRUC PSUGF30HF 填料,玻璃纤维增强材料,30%填料按重量.
美国RTP PPS RTP 1300 AR 15 TFE 15 SI 2 填料,芳族聚酰胺纤维,15%填料按重量.
德国赢创(德固赛) PEEK VESTAKEEP® 4000G
日本宝理 LCP LAPEROS® E477i 填料,Polyplastics,日本宝理.
俄罗斯Poly Plastic POM均聚 Technacet® A-110
● EVA 韩国现代 VS410 其它
● EVA 日本住友 MB-11
VAC含量32%
● EVA 美国杜邦 Elvax 3128-1
● EVA 乐天化学 VA600
工艺性、粘合性
● EVA 三星道达尔 E201
良好的加工性能,耐低温,抗冲击性高,ESCR