性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
比重 | ASTMD792 | 1.07 | g/cm3 | |
肖氏硬度 | 邵氏A,100°C | ASTMD2240 | 80 | |
肖氏硬度 | 邵氏A,24°C2 | ASTMD2240 | 80 | |
肖氏硬度 | 邵氏A,24°C3 | ASTMD2240 | 75 | |
拉伸应力 | 100%应变,24°C2 | ASTMD412 | 2.76 | MPa |
拉伸应力 | 100%应变,24°C3 | ASTMD412 | 2.59 | MPa |
拉伸应力 | 100%应变,100°C | ASTMD412 | 2.76 | MPa |
拉伸应力 | 300%应变,24°C2 | ASTMD412 | 4.31 | MPa |
拉伸应力 | 300%应变,24°C3 | ASTMD412 | 3.79 | MPa |
拉伸应力 | 300%应变,100°C | ASTMD412 | 4.31 | MPa |
抗张强度 | 24°C2 | ASTMD412 | 20.7 | MPa |
抗张强度 | 24°C3 | ASTMD412 | 17.9 | MPa |
抗张强度 | 100°C | ASTMD412 | 11.7 | MPa |
伸长率 | 断裂,100°C | ASTMD412 | 650 | % |
伸长率 | 断裂,24°C2 | ASTMD412 | 800 | % |
伸长率 | 断裂,24°C3 | ASTMD412 | 780 | % |
撕裂强度 | 开裂4 | ASTMD470 | 5.3 | kN/m |
撕裂强度 | 开裂3 | ASTMD470 | 11 | kN/m |
撕裂强度 | 开裂2 | ASTMD470 | 12 | kN/m |
压缩永久变形(70°C,22hr) | ASTMD395B | 45 | % | |
巴肖氏弹性 | ASTMD2632 | 70 | % | |
体积变化 | 50°C,168hr5 | ASTMD471 | 180 | % |
体积变化 | 50°C,168hr,ASTM标准油(3号) | ASTMD471 | 25 | % |
体积变化 | 50°C,168hr,在基准燃料B中 | ASTMD471 | 60 | % |
体积变化 | 50°C,168hr,在甲乙酮中 | ASTMD471 | 500 | % |
热固组件 | 树脂 | 按重量计算的混合比:100 | ||
热固组件 | 硬化法 | 按重量计算的混合比:8.8 | ||
热固组件 | 储存稳定性(100°C) | 6.0到12 | min | |
热固组件 | 脱模时间(100°C) | 45到60 | min | |
热固组件 | 后固化时间(24°C) | 170 | hr | |
AbrasionIndex-NBS | 110 | |||
固化时间(100°C) | 3.0 | hr |
PUR脂肪族 L 42塑料供应商,长期销售美国科聚亚生产的PUR脂肪族原料,以上是“PUR脂肪族 TDI/Adiprene® L 42”塑胶料的物性表参数.近期代理商可转仓交易:法国AD MAJORIS PP MAJORIS EW300
美国Honeywell PCTFE ACLAR® 33C (7.8 mil)
土耳其Elastron TPV Elastron® V P.V101.A65.B 可粘结性,柔软,挤出,注射成型 医疗/护理用品
日本美拉龙 TPU合金 Mirakutoran® TPU E670MNAT
中国南通普力马 TPE Maxelast® P3660T 包覆成型
德国巴斯夫 TPU聚脂 Elastollan® C 74 D
意大利API TPU聚醚 apilon 52® TL 40 可回收材料,抗微生物,耐油性能,耐低温良好,耐磨损性,耐水解性,注射成型 体育用品,电器用具,垫圈,涂层应用,电气/电子应用领域,鞋类,家用货品,车轮,管件,传送带修补,动力/其它工具,把手
德国凯柏胶宝 TPE THERMOLAST® K TP5VCN (Series: AD1/CS)
美国Teknor Apex TPE Medalist™ MD-53263 (PRELIMINARY DATA)
台湾台橡Dexco SBS VECTOR® 2518A
中国东莞顶塑 TPE Topolymer® 8201-B