性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
比重 | ASTMD792 | 1.85 | g/cm3 | |
门尼粘度(ML1+10,121°C) | ASTMD1646 | 65 | MU | |
肖氏硬度 | 邵氏A,23°C | ASTMD2240 | 68 | |
肖氏硬度 | 邵氏A,23°C2 | ASTMD2240 | 72 | |
肖氏硬度 | 邵氏A,23°C3 | ASTMD2240 | 70 | |
肖氏硬度 | 邵氏A,23°C4 | ASTMD2240 | 72 | |
肖氏硬度 | 邵氏A,23°C5 | ASTMD2240 | 70 | |
TensileStress(10%Strain) | 23°C6 | ASTMD412 | 0.800 | MPa |
TensileStress(10%Strain) | 23°C7 | ASTMD412 | 0.900 | MPa |
拉伸应力 | 100%应变,23°C8 | ASTMD412 | 4.20 | MPa |
拉伸应力 | 100%应变,23°C9 | ASTMD412 | 5.10 | MPa |
拉伸应力 | 100%应变,23°C10 | ASTMD412 | 5.00 | MPa |
拉伸应力 | 100%应变,23°C11 | ASTMD412 | 4.30 | MPa |
拉伸应力 | 100%应变,23°C12 | ASTMD412 | 3.20 | MPa |
抗张强度 | 屈服,23°C8 | ASTMD412 | 12.7 | MPa |
抗张强度 | 屈服,23°C9 | ASTMD412 | 9.90 | MPa |
抗张强度 | 屈服,23°C10 | ASTMD412 | 16.5 | MPa |
抗张强度 | 屈服,23°C11 | ASTMD412 | 14.1 | MPa |
抗张强度 | 屈服,23°C12 | ASTMD412 | 12.3 | MPa |
伸长率 | 断裂,23°C8 | ASTMD412 | 230 | % |
伸长率 | 断裂,23°C9 | ASTMD412 | 150 | % |
伸长率 | 断裂,23°C10 | ASTMD412 | 220 | % |
伸长率 | 断裂,23°C11 | ASTMD412 | 260 | % |
伸长率 | 断裂,23°C12 | ASTMD412 | 310 | % |
压缩永久变形(200°C,22hr) | ASTMD395B | 17 | % | |
体积变化 | 23°C,168hr,C级标准燃料 | ASTMD471 | 6.7 | % |
体积变化 | 23°C,168hr,inM15(FuelC/Methanol85/15) | ASTMD471 | 19 | % |
体积变化 | 23°C,168hr,甲醇 | ASTMD471 | 18 | % |
体积变化 | 150°C,168hr,在ASTM105油中 | ASTMD471 | 0.80 | % |
氟橡胶 GBLT-600S塑料供应商,长期销售美国科慕化学生产的氟橡胶原料,以上是“氟橡胶 Viton® GBLT-600S”塑胶料的物性表参数.近期代理商可转仓交易:Generic 酚醛 Generic Phenolic - Glass Fiber,S-Glass 填料,高强度玻璃纤维.
美国APS TPV Viprene™ P70A-22U-NAT 良好的流动性,抗紫外线性能良好,热稳定性,挤出,注射成型
中国深圳盛嘉伦 TPE Gallonprene® GP420-3502 高光,无卤,可喷涂的,注射成型 玩具,包覆成型,柔软的把手
日本美拉龙 TPU合金 Mirakutoran® TPU H885FNAT
奥地利北欧化工 TPO Daplen™ EE103AEB 填料,矿物填料,10%填料按重量.汽车防撞杆,汽车领域的应用,汽车外部装饰
日本三菱 TPE tefabloc® TP SD 333 45A 抗紫外线性能良好,耐洗涤剂,耐碱,耐化学性良好,食品接触的合规性,耐酸,流动性高,优良外观,注射成型 体育用品,室外应用,玩具,密封件
中国深圳盛嘉伦 TPE Gallonprene® GP100-7002 可喷涂的,无卤,高光,注射成型 玩具,包覆成型,柔软的把手
英国ELASTO SEBS Dryflex® 602850S
土耳其Elastron SBS Elastron® D D100.A30.B 柔软,嵌段共聚物,可粘结性,注射成型