性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
比重 | ASTMD792 | 1.82 | g/cm3 | |
表观密度 | ASTMD1895 | 1.82 | g/cm3 | |
门尼粘度(ML1+10,121°C) | ASTMD1646 | 65 | MU | |
肖氏硬度 | 邵氏A,23°C | ASTMD2240 | 71 | |
肖氏硬度 | 邵氏A,23°C2 | ASTMD2240 | 75 | |
肖氏硬度 | 邵氏A,23°C3 | ASTMD2240 | 72 | |
肖氏硬度 | 邵氏A,23°C4 | ASTMD2240 | 77 | |
肖氏硬度 | 邵氏A,23°C5 | ASTMD2240 | 76 | |
拉伸应力 | 100%应变,23°C6 | ASTMD412 | 3.10 | MPa |
拉伸应力 | 100%应变,23°C7 | ASTMD412 | 4.60 | MPa |
拉伸应力 | 100%应变,23°C8 | ASTMD412 | 4.50 | MPa |
拉伸应力 | 100%应变,23°C9 | ASTMD412 | 4.50 | MPa |
拉伸应力 | 100%应变,23°C10 | ASTMD412 | 4.90 | MPa |
抗张强度 | 屈服,23°C6 | ASTMD412 | 9.70 | MPa |
抗张强度 | 屈服,23°C7 | ASTMD412 | 14.5 | MPa |
抗张强度 | 屈服,23°C8 | ASTMD412 | 15.0 | MPa |
抗张强度 | 屈服,23°C9 | ASTMD412 | 13.5 | MPa |
抗张强度 | 屈服,23°C10 | ASTMD412 | 14.1 | MPa |
伸长率 | 断裂,23°C6 | ASTMD412 | 350 | % |
伸长率 | 断裂,23°C7 | ASTMD412 | 240 | % |
伸长率 | 断裂,23°C8 | ASTMD412 | 260 | % |
伸长率 | 断裂,23°C9 | ASTMD412 | 240 | % |
伸长率 | 断裂,23°C10 | ASTMD412 | 230 | % |
压缩永久变形 | 23°C,70hr | ASTMD395B | 18 | % |
压缩永久变形 | 200°C,70hr | ASTMD395B | 21 | % |
压缩永久变形 | 200°C,168hr | ASTMD395B | 29 | % |
压缩永久变形 | 232°C,70hr | ASTMD395B | 40 | % |
氟橡胶 A-331C塑料供应商,长期销售美国科慕化学生产的氟橡胶原料,以上是“氟橡胶 Viton® A-331C”塑胶料的物性表参数.近期代理商可转仓交易:德国特尔 PP TEREZ PA/PP 7500 GF 30 填料,玻璃纤维增强材料,30%填料按重量.
日本京瓷 酚醛 TECOLITE KM-450(J)
美国Greene PFE Chemraz 629 纯度高,高弹性 密封件,阀门/阀门部件
意大利Taro Plast TPV TAROPRENE® 2 A65 E1G 脱模性能良好,流动性高 外壳
日本美拉龙 TPU合金 Mirakutoran® TPU E498
中国江苏鼎启钟华 TPE Jiangsu Sinarise PX900M 电线电缆应用
韩国LG化学 TPO Lupol® HI5204H 填料,矿物填料,20%填料按重量.汽车内部零件
墨西哥化工 TPE Garaflex™ G 7782-A4 挤出 软线护套
比利时Ravago TPE ENFLEX S3015A 抗溶剂性,耐油性能,高耐热性,良好的着色性,可回收材料,耐碱,耐酸,可加工性良好,良好粘结性,耐臭氧性能,耐酒精,抗紫外线性能良好,低的压缩变形性,耐洗涤剂,高弹性,注射成型,挤出
英国ELASTO SEBS Dryflex® A2 500350
墨西哥化工 SBS Evoprene™ 029