性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
比重 | ASTMD792 | 1.82 | g/cm3 | |
门尼粘度(ML1+10,121°C) | ASTMD1646 | 100 | MU | |
肖氏硬度 | 邵氏A,23°C | ASTMD2240 | 77 | |
肖氏硬度 | 邵氏A,23°C2 | ASTMD2240 | 77 | |
肖氏硬度 | 邵氏A,23°C3 | ASTMD2240 | 77 | |
肖氏硬度 | 邵氏A,23°C4 | ASTMD2240 | 77 | |
肖氏硬度 | 邵氏A,23°C5 | ASTMD2240 | 77 | |
拉伸应力 | 100%应变,23°C6 | ASTMD412 | 7.90 | MPa |
拉伸应力 | 100%应变,23°C7 | ASTMD412 | 7.80 | MPa |
拉伸应力 | 100%应变,23°C8 | ASTMD412 | 7.70 | MPa |
拉伸应力 | 100%应变,23°C9 | ASTMD412 | 6.90 | MPa |
拉伸应力 | 100%应变,23°C10 | ASTMD412 | 5.60 | MPa |
抗张强度 | 屈服,23°C6 | ASTMD412 | 16.0 | MPa |
抗张强度 | 屈服,23°C7 | ASTMD412 | 14.7 | MPa |
抗张强度 | 屈服,23°C8 | ASTMD412 | 13.8 | MPa |
抗张强度 | 屈服,23°C9 | ASTMD412 | 13.9 | MPa |
抗张强度 | 屈服,23°C10 | ASTMD412 | 10.6 | MPa |
伸长率 | 断裂,23°C6 | ASTMD412 | 190 | % |
伸长率 | 断裂,23°C7 | ASTMD412 | 180 | % |
伸长率 | 断裂,23°C8 | ASTMD412 | 170 | % |
伸长率 | 断裂,23°C9 | ASTMD412 | 170 | % |
伸长率 | 断裂,23°C10 | ASTMD412 | 180 | % |
压缩永久变形 | 23°C,70hr | ASTMD395B | 6.0 | % |
压缩永久变形 | 200°C,22hr | ASTMD395B | 6.0到11 | % |
压缩永久变形 | 200°C,70hr | ASTMD395B | 20 | % |
压缩永久变形 | 200°C,168hr | ASTMD395B | 29 | % |
压缩永久变形 | 232°C,70hr | ASTMD395B | 36 | % |
氟橡胶 A-601C塑料供应商,长期销售美国科慕化学生产的氟橡胶原料,以上是“氟橡胶 Viton® A-601C”塑胶料的物性表参数.近期代理商可转仓交易:美国福禄 PP GAPEX® RPP30EA52WH 抗氧化性,共聚物,挤出涂层 汽车领域的应用,粘合剂,涂层应用
奥地利北欧化工 PP Fibremod™ GB215HP
比利时索尔维 PVDF Solef® 60512 粘度高,共聚物 管道系统
芬兰普宓斯 TPU PRE-ELEC® TPU 1511
英国ELASTO TPV Dryflex® 51395 V
德国凯柏胶宝 TPE For-Tec E OC6OAZ (Series: AD/PAX/CR)
英国Aurora Manufacturing TPO AURAPENE PPTF20BK 填料,滑石填料,20%填料按重量.通用
美国普立万 TPE Dynalloy™ OBC8000-T05 良好的流动性,良好的加工稳定性,良好的着色性,柔软,硬度,低,注射成型 透明或半透明配件,包覆成型,密封件,柔软的把手,消费品应用领域,个人护理
美国Teknor Apex TPE Telcar® TL-1343A BLK 111
美国普立万 TPE Versalloy™ XL 9070X-9 可回收材料,良好的流动性,优良外观,注射成型 消费品应用领域,薄壁部件,包覆成型,柔软触感应用
土耳其Elastron SEBS Elastron® G G500.A50.N.ABS 良好的着色性,柔软,良好粘结性,可粘结性,嵌段共聚物,注射成型