流动性高,抗撞击性,高 | 不透明 |
电器用具 | |
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
比重 | ASTMD792 | 1.33 | g/cm3 | |
SpiralFlow | 102 | cm | ||
收缩率-流动 | ASTMD955 | 0.20到0.50 | % | |
肖氏硬度(邵氏D) | ASTMD2240 | 79 | ||
拉伸模量2 | ASTMD638 | 2590 | MPa | |
抗张强度2(屈服) | ASTMD638 | 41.4 | MPa | |
伸长率2(断裂) | ASTMD638 | 35 | % | |
弯曲模量 | ASTMD790 | 2410 | MPa | |
弯曲强度 | ASTMD790 | 67.6 | MPa | |
悬壁梁缺口冲击强度 | -18°C,3.18mm,注塑 | ASTMD256A | 160 | J/m |
悬壁梁缺口冲击强度 | 0°C,3.18mm,注塑 | ASTMD256A | 210 | J/m |
悬壁梁缺口冲击强度 | 23°C,3.18mm,注塑 | ASTMD256A | 800 | J/m |
载荷下热变形温度 | 0.45MPa,未退火,3.18mm | ASTMD648 | 72.2 | °C |
载荷下热变形温度 | 0.45MPa,退火,3.18mm | ASTMD648 | 70.0 | °C |
载荷下热变形温度 | 1.8MPa,未退火,6.35mm | ASTMD648 | 68.9 | °C |
载荷下热变形温度 | 1.8MPa,退火,6.35mm | ASTMD648 | 72.8 | °C |
RTIElec | UL746 | 90.0 | °C | |
RTIImp | UL746 | 85.0 | °C | |
RTI | UL746 | 90.0 | °C | |
UL阻燃等级 | 1.4mm,ALL | UL94 | V-0 | |
UL阻燃等级 | 1.6mm,ALL | UL94 | 5VA | |
CSA可燃性3(1.60mm) | V-05VA |
pvc刚硬 Vinyl Rigid Molding M3880塑料供应商,长期销售美国普立万生产的pvc刚硬原料,以上是“pvc刚硬 Geon™ Vinyl Rigid Molding M3880”塑胶料的物性表参数.近期代理商可转仓交易:德国巴斯夫 PA6 Miramid® VET30C 填料,玻璃纤维增强材料,30%填料按重量.工程配件,体育用品
美国RTP PA612 RTP 205 D 填料,玻璃纤维增强材料,30%填料按重量.
斯洛伐克Plastcom PA6 SLOVAMID® 6 GF 15 MI/2
美国特诺尔爱佩斯 pvc易弯曲 Vital-Line SHE2008X 屏蔽,X,射线,挤出 医疗/护理用品
美国普立万 pvc易弯曲 Geon™ Vinyl Flexible A9001 高光,通用,注射成型,挤出 管件,薄膜,片材,管道,通用
美国Colorite pvc刚硬 Colorite Rigid PVC 2503 抗撞击性高,流动性高,耐气候影响性能良好,热稳定性,清晰度高,高光,注射成型 通用,室外应用
澳大利亚PolyPacific PP Retpol® 7025/4 UV3
韩国LG化学 PP均聚 SEETEC PP H5300
● pvc刚硬 美国Axiall Axiall PVC 8607
抗撞击性高,高刚性型材挤出成型
● pvc刚硬 美国Teknor Apex APEX RS 8216
高光,抗撞击性高
● pvc刚硬 美国威凯 Vi-Chem PVC VSR87-80E
填料:Vi-Chem 美国威凯。
● pvc刚硬 美国Teknor Apex APEX RE 8003
抗撞击性高,光泽中,挤出
● pvc刚硬 美国Axiall Axiall PVC 9113
高刚性,抗撞击性高,吹塑成型