延高的拉伸率,刚性,高 注射成型 | |
填料:玻璃纤维增强材料, 40% 填料按重量。 |
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
比重 | ASTMD792 | 1.30 | g/cm3 | |
熔流率(熔体流动速率)(260°C/5.0kg) | ASTMD1238 | 1.3 | g/10min | |
收缩率-流动(3.20mm) | InternalMethod | 0.17to0.18 | % | |
MoldingShrinkage-AcrossFlow(3.20mm) | InternalMethod | 0.27to0.61 | % | |
抗张强度2(屈服) | ASTMD638 | 95.8 | MPa | |
抗张强度2(断裂) | ASTMD638 | 95.8 | MPa | |
伸长率2(断裂) | ASTMD638 | 6.4 | % | |
弯曲模量4(50.0mm跨距) | ASTMD790 | 8320 | MPa | |
FlexuralStrength3(Break,50.0mmSpan) | ASTMD790 | 151 | MPa | |
悬壁梁缺口冲击强度 | -30°C | ASTMD256 | 96 | J/m |
悬壁梁缺口冲击强度 | 23°C | ASTMD256 | 110 | J/m |
悬壁梁缺口冲击强度(23°C) | ASTMD4812 | 580 | J/m | |
装有测量仪表的落镖冲击 | -30°C,TotalEnergy | ASTMD3763 | 14.1 | J |
装有测量仪表的落镖冲击 | 23°C,TotalEnergy | ASTMD3763 | 16.8 | J |
载荷下热变形温度(0.45MPa,未退火,3.20mm) | ASTMD648 | 159 | °C | |
载荷下热变形温度(1.8MPa,未退火,3.20mm) | ASTMD648 | 146 | °C | |
维卡软化温度 | ASTMD15254 | 163 | °C | |
线形热膨胀系数-流动(-40到40°C) | ASTME831 | 1.1E-5 | cm/cm/°C | |
线形热膨胀系数-横向(-40到40°C) | ASTME831 | 6.3E-5 | cm/cm/°C |
PPO(PPE) PPX640 resin塑料供应商,长期销售沙伯基础生产的PPO(PPE)原料,以上是“PPO(PPE) NORYL™ PPX640 resin”塑胶料的物性表参数.近期代理商可转仓交易:韩国LG化学 TPO Lupol® TE5104 填料,矿物填料.汽车外部零件
比利时Ravago TPV ENFLEX V1070A
德国巴斯夫 TPU聚脂 Elastollan® L 785 A
德国凯柏胶宝 TPE THERMOLAST® K TF1STL (Series: FC/S)
美国Kraton SEBS KRATON® A1535 H
印度ENPLAST TPE ENSOFT SO-160-55A 抗紫外线性能良好,耐臭氧性能,注射成型,挤出
美国狮王 EPDM Royaltherm® 1721
美国埃克森美孚化工 EVA Escorene™ Ultra LD 730.09 Molding
美国RTP PPA RTP 4099 X 105534 耐磨损性良好,注射成型
美国塞拉尼斯 PPS Fortron® 4332L6
沙伯基础 PEI ULTEM™ PW2300 resin
美国QTR PC QR Resin QR-1235P 可电镀,高耐热性,抗撞击性良好,耐低温冲击,脱模性能良好
意大利拉题 POM共聚 Latilub 73/13 Y/20 填料,芳族聚酰胺纤维,20%填料按重量.
美国杜邦 POM均聚 Delrin® 500TL NC010 耐磨损性良好,中等粘性,低摩擦系数,润滑,注射成型
沙伯基础 PC LNP™ LUBRICOMP™ DP003 compound